Paremeters Technical kanggo meneng kembar podo lan tong minyak
Bahan Baja 38GrMoAlA,42GrMo
Kekerasan sawise hardening & tempering HB: 280-320
Hardness & Tempering wektu 72 jam
Nitrided atose HV: 850-1000
Nitrided wektu 120 jam
Ambane kasus nitriding 0,50-0,80mm
Nitrided Brittleness kurang saka kelas 2
Kekasaran lumahing Ra: 0.4
atose lumahing kromium-plating sawise Nitriding>HV900
Ambane kromium -plating 0.025-0.10mm
Alloy atose HRC: 50-65
Alloy ambane 0.8-2.0mm
Aplikasi:
PE, PP, ABS, karet, macem-macem serat kaca dhuwur, serat mineral lan PPA, PPS, PA6T, LCP, VO proteksi geni, daya ferrous, bubuk Magnetik, etc.
Kanggo bahan plastik recycled, PVC + 30% CaCo3, etc